SLTC 2026 CONFERENCE 24TH-25TH APRIL – SAVE THE DATE
Abstract
Previous studies indicated that Cr( VI) was not detected or was below 5 mg/kg in tanned leather scraps. However, after they are burned, the resulting ashes contain meaningfu] amounts of Cr(VI) that depend on the burning temperature. Furthermore, results obtained at the same ignition temperature, but different holding times, show high variability. 3 This paper presents experimental results that confirm the Cr(II1) to Cr(VI) transformation during chromium tanned leather combustion and its dependence on temperature and time, thus finding an explanation for variability of the results published before.
£20.00